Nimonic 90
Age-hardenable Ni-Cr-Co alloy for turbine blades and high-temperature springs to 920°C.
Introduction
§01, General80A with more muscle. Nimonic 90 raises titanium and aluminum and adds cobalt, which lifts the gamma-prime solvus and extends useful creep strength to 920°C. Hot-section blades, discs and high-temperature springs take advantage, and at 8.18 g/cm³ it's slightly lighter than its predecessor too.
Cross-Reference
Quick Facts
- UNS
- N07090
- GB
- GH4090
- Density
- 8.18 g/cm³
- Max Service Temp
- 920°C
- Series
- Nimonic
Chemical Composition
ASTM B637 / AMS 5829 (N07090), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | Balance | Base matrix |
| Chromium | Cr | 18.0 – 21.0 | Oxidation resistance |
| Cobalt | Co | 15.0 – 21.0 | Phase stability & hot strength |
| Titanium | Ti | 2.0 – 3.0 | γ′ age hardening |
| Aluminum | Al | 1.0 – 2.0 | γ′ age hardening |
| Carbon | C | 0.13 max | Carbide control |
| Iron | Fe | 5.0 max | Controlled residual |
Mechanical & Physical Properties
Manufacturer datasheet, typical (aged)
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | ≈1050 MPa | Typical, aged bar RT |
| Yield Strength (0.2% offset) | ≈750 MPa | Typical, aged bar RT |
| Elongation | ≈20% | Typical, aged bar RT |
| Density | 8.18 g/cm³ | Physical |
Applicable Standards & Product Forms
Nimonic 90 · UNS N07090 · GB/T GH4090
| Standard | Product Form |
|---|---|
| ASTM B637 | Bar & forgings |
| BS HR 202 | Sheet & bar (UK) |
| AMS 5829 | Bar & forgings |
| DIN 17742 | Cross-reference designation |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Nimonic Grades
Rated 815°C, lower than this grade, also used for automotive, same Nimonic series.
Rated 750°C, lower than this grade, also used for turbine, same Nimonic series.
Rated 1000°C, higher than this grade, also used for turbine, same Nimonic series.
Related Nickel Alloys
Rated 870°C, in the same class as this grade, also used for aerospace, from the Waspaloy series.
Rated 870°C, in the same class as this grade, also used for fasteners, from the Waspaloy series.
Rated 700°C, lower than this grade, also used for turbocharger, from the Incoloy series.
Pricing
How Nimonic 90 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Nimonic 90 FAQWhat is Nimonic 90 used for?
Nimonic 90 is a Nimonic alloy used in Gas turbine hot-section blades, Turbine discs and rings, High-temperature springs to 920°C. It offers 920°C creep strength and Cobalt-enhanced gamma-prime.
What is the chemical composition of Nimonic 90?
Nimonic 90 is a controlled-composition Nimonic alloy supplied to ASTM B637 and BS HR 202. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Nimonic 90 available in?
Nimonic 90 is regularly supplied in Forging, Wire, Spring Wire, Bar & Rod, Plate & Sheet. Custom forms and dimensions available on request.
What is the maximum service temperature of Nimonic 90?
Nimonic 90 is rated for service up to 920°C. Contact our metallurgy team for specific application recommendations.
Need Nimonic 90 material?
Request a quote with your specification: grade, form, dimensions and quantity.