§01, General

An 80/20 nickel-chromium base with a little titanium for precipitation strengthening. Nimonic 75 oxidizes slowly at combustion temperatures and forms into sheet hardware without drama, which is why gas turbine combustion chambers, heat-treatment fixtures and furnace parts still consume it in volume.

Cross-Reference

UNS: UNS N06075
GB/T: GB GH3030
Series: Nimonic
Density: 8.37 g/cm³
Max Temp: 1000°C
Standards: ASTM B637 · BS HR 5 · DIN 17742

Quick Facts

UNS
N06075
GB
GH3030
Density
8.37 g/cm³
Max Service Temp
1000°C
Series
Nimonic

Chemical Composition

ASTM B637 / DIN 17742 (N06075), wt%

Element Symbol Content (wt%) Role
Nickel Ni Balance Base matrix
Chromium Cr 18.0 – 21.0 Oxidation resistance
Titanium Ti 0.2 – 0.6 Minor carbide/γ′ control
Iron Fe 5.0 max Controlled residual
Carbon C 0.08 – 0.15 Carbide strengthening
Manganese Mn 1.0 max Deoxidiser
Silicon Si 1.0 max Controlled residual

Mechanical & Physical Properties

Manufacturer datasheet, typical (annealed)

Property Value Condition
Tensile Strength 600 MPa Typical, annealed RT
Yield Strength (0.2% offset) 300 MPa Typical, annealed RT
Elongation 35% Typical, annealed RT
Density 8.37 g/cm³ Physical

Applicable Standards & Product Forms

Nimonic 75 · UNS N06075 · GB/T GH3030

Standard Product Form
ASTM B637 Bar & forgings
BS HR 5 Sheet & strip (UK)
DIN 17742 Cross-reference designation
ForgingWireBar & RodPlate & SheetStrip

Available Product Forms

§02, Forms
ForgingWireBar & RodPlate & SheetStrip

Key Characteristics

§03, Features
Good oxidation resistance to 1000°C
Sheet metal-capable
Ti precipitation-strengthened
Weldable
Cost-effective 80/20 Ni-Cr base

Typical Uses

§04, Applications
Gas turbine combustion chambers
Heat-treatment furnace fixtures
Industrial oven components
Sheet metal fabrications
Exhaust system components

Pricing

How Nimonic 75 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

Nimonic 75 FAQ

What is Nimonic 75 used for?

Nimonic 75 is a Nimonic alloy used in Gas turbine combustion chambers, Heat-treatment furnace fixtures, Industrial oven components. It offers Good oxidation resistance to 1000°C and Sheet metal-capable.

What is the chemical composition of Nimonic 75?

Nimonic 75 is a controlled-composition Nimonic alloy supplied to ASTM B637 and BS HR 5. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is Nimonic 75 available in?

Nimonic 75 is regularly supplied in Forging, Wire, Bar & Rod, Plate & Sheet, Strip. Custom forms and dimensions available on request.

What is the maximum service temperature of Nimonic 75?

Nimonic 75 is rated for service up to 1000°C. Contact our metallurgy team for specific application recommendations.

Need Nimonic 75 material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google