GH3044 alloy products
Material Family / Waspaloy

GH3044

Ni-Cr-W alloy for sheet metal gas turbine hot-section and industrial furnace components.

Introduction

§01, General

Sheet metal that survives the hot section. GH3044 is a solid-solution Ni-Cr-W alloy with good oxidation resistance and moderate strength at gas turbine and industrial furnace temperatures, and it forms and welds without a fight. Complex sheet assemblies come out of it readily, which is exactly what a fabricator needs at 900°C-class duty.

Cross-Reference

UNS: UNS N06604
Series: Waspaloy
Density: 8.89 g/cm³
Max Temp: 900°C
Standards: GB/T 14994 · ASTM B435 equivalent

Quick Facts

UNS
N06604
Density
8.89 g/cm³
Max Service Temp
900°C
Series
Waspaloy

Chemical Composition

GB/T 14992, GH3044 (Ni-Cr-W), nominal wt%

Element Symbol Content (wt%) Role
Nickel Ni Balance Base
Chromium Cr 23.5 – 26.5 Oxidation resistance
Tungsten W 14.5 – 16.0 Solid-solution strengthening
Iron Fe 4.0 max Controlled residual
Aluminum Al 0.5 max Controlled residual
Titanium Ti 0.5 max Controlled residual
Carbon C 0.10 max Controlled residual

Mechanical & Physical Properties

GB literature, typical (sheet, solution treated)

Property Value Condition
Tensile Strength (RT) ≈735 MPa min Typical, sheet
Max Service Temperature 900 °C Oxidising atmosphere
Density 8.89 g/cm³ Physical

Applicable Standards & Product Forms

GH3044 · UNS N06604 · GB/T GH3044

Standard Product Form
GB/T 14992 Sheet / bar / forging
Plate & SheetBar & RodForgingPipe & Tube

Available Product Forms

§02, Forms
ForgingWireBar & RodPlate & SheetStripPipe & Tube

Key Characteristics

§03, Features
Sheet metal-optimized
Good formability
Weldable
900°C oxidation resistance
Solid-solution strengthened

Typical Uses

§04, Applications
Gas turbine hot-section sheet metal
Industrial furnace muffles and retorts
Heat-treatment baskets and fixtures
Aircraft exhaust components
Combustion can assemblies

Selection guide

GH3044 vs Inconel 625 vs Hastelloy X

Three nickel-chromium alloys that get quoted against each other constantly. The tungsten, molybdenum and niobium lines explain which duty points at which one.

Compare the three →

Pricing

How GH3044 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

GH3044 FAQ

What is GH3044 used for?

GH3044 is a Waspaloy alloy used in Gas turbine hot-section sheet metal, Industrial furnace muffles and retorts, Heat-treatment baskets and fixtures. It offers Sheet metal-optimized and Good formability.

What is the chemical composition of GH3044?

GH3044 is a controlled-composition Waspaloy alloy supplied to GB/T 14994 and ASTM B435 equivalent. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is GH3044 available in?

GH3044 is regularly supplied in Forging, Wire, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube. Custom forms and dimensions available on request.

What is the maximum service temperature of GH3044?

GH3044 is rated for service up to 900°C. Contact our metallurgy team for specific application recommendations.

Need GH3044 material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google