Introduction
§01, GeneralFrom 650°C to 870°C, Waspaloy keeps creep-rupture strength through the thermal cycles that age lesser alloys out. The precipitation-hardened Ni-Cr-Co chemistry was developed for aircraft gas turbine discs, rings and shafts, and it still holds oxidation resistance and microstructural stability cycle after cycle.
Cross-Reference
Quick Facts
- UNS
- N07001
- GB
- GH4738
- Density
- 8.22 g/cm³
- Max Service Temp
- 870°C
- Series
- Waspaloy
Chemical Composition
AMS 5708 / ASTM B637 (N07001), wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Nickel | Ni | Balance (≈57) | Base matrix |
| Chromium | Cr | 18.0 – 21.0 | Oxidation resistance |
| Cobalt | Co | 12.0 – 15.0 | Phase stability & hot strength |
| Molybdenum | Mo | 3.5 – 5.0 | Strengthening |
| Titanium | Ti | 2.75 – 3.25 | γ′ age hardening |
| Aluminum | Al | 1.2 – 1.6 | γ′ age hardening |
| Iron | Fe | 2.0 max | Controlled residual |
| Carbon | C | 0.05 – 0.12 | Carbide control |
| Boron | B | 0.003 – 0.010 | Grain boundary control |
| Zirconium | Zr | 0.02 – 0.08 | Grain boundary control |
Mechanical & Physical Properties
Manufacturer datasheet, typical (aged)
| Property | Value | Condition |
|---|---|---|
| Tensile Strength | ≈1050 MPa | Typical, aged bar RT |
| Yield Strength (0.2% offset) | ≈760 MPa | Typical, aged bar RT |
| Elongation | ≈18% | Typical, aged bar RT |
| Density | 8.22 g/cm³ | Physical |
Applicable Standards & Product Forms
Waspaloy · UNS N07001 · GB/T GH4738
| Standard | Product Form |
|---|---|
| AMS 5708 | Bar (aged) |
| AMS 5709 | Bar |
| AMS 5544 | Sheet & strip |
| ASTM B637 | Bar & forgings |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Waspaloy Grades
Rated 870°C, in the same class as this grade, also used for structural, same Waspaloy series.
Rated 1000°C, higher than this grade, also used for aircraft, same Waspaloy series.
Rated 900°C, in the same class as this grade, also used for aircraft, same Waspaloy series.
Rated 1000°C, higher than this grade, also used for aircraft, same Waspaloy series.
Related Nickel Alloys
Rated 750°C, lower than this grade, also used for compressor, from the Nimonic series.
Rated 920°C, in the same class as this grade, also used for fasteners, from the Nimonic series.
Rated 700°C, lower than this grade, also used for fasteners, from the Incoloy series.
Pricing
How Waspaloy is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
Waspaloy FAQWhat is Waspaloy used for?
Waspaloy is a Waspaloy alloy used in Turbine discs and rings, Compressor shafts, High-temperature fasteners. It offers Exceptional creep-rupture strength to 870°C and Precipitation-hardenable for turbine applications.
What is the chemical composition of Waspaloy?
Waspaloy is a controlled-composition Waspaloy alloy supplied to AMS 5708 and AMS 5709. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is Waspaloy available in?
Waspaloy is regularly supplied in Forging, Wire, Flange, Bar & Rod, Plate & Sheet, Strip. Custom forms and dimensions available on request.
What is the maximum service temperature of Waspaloy?
Waspaloy is rated for service up to 870°C. Contact our metallurgy team for specific application recommendations.