GH4098 alloy products
Material Family / Waspaloy

GH4098

High-chromium Ni-based alloy for sheet metal combustion chamber and afterburner components.

Introduction

§01, General

Chromium does the work here. GH4098 is a high-chromium Chinese nickel superalloy built for sheet fabrication of combustion chambers, afterburner components and thermal protection systems, with oxidation resistance that covers intermittent service to 1000°C. Thin gauge, hot gas, repeated cycles: that's its home turf.

GB/T 14994

Quick Facts

Density
8.3 g/cm³
Max Service Temp
1000°C
Series
Waspaloy

Chemical Composition

GB/T 14992, GH4098 (Ni-Cr-Co-Mo-W-Al-Ti), nominal wt% — verify before publish

Element Symbol Content (wt%) Role
Nickel Ni Balance Base
Chromium Cr 11.0 – 13.0 Oxidation resistance
Cobalt Co 9.5 – 11.5 Phase stability
Molybdenum Mo 4.5 – 5.5 Strengthening
Tungsten W 4.5 – 5.5 Strengthening
Aluminum Al 2.5 – 3.2 γ′ forming
Titanium Ti 2.3 – 3.0 γ′ forming
Carbon C 0.10 max Controlled residual

Mechanical & Physical Properties

GB literature, typical (aged)

Property Value Condition
Tensile Strength (RT) ≈1200 MPa Typical, aged
Max Service Temperature 1000 °C Turbine blade/vane duty
Density 8.3 g/cm³ Physical

Applicable Standards & Product Forms

GH4098 · UNS — · GB/T GH4098

Standard Product Form
GB/T 14992 Bar / forging / blade stock
Bar & RodForgingWire

Available Product Forms

§02, Forms
ForgingWireBar & RodPlate & SheetStrip

Key Characteristics

§03, Features
1000°C intermittent service
Sheet metal fabricable
High chromium oxidation resistance
Afterburner qualified
Chinese aerospace standard

Typical Uses

§04, Applications
Aircraft afterburner components
Combustion chamber liners
Thermal protection panels
Missile exhaust components
High-temperature sheet metal

Pricing

How GH4098 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

GH4098 FAQ

What is GH4098 used for?

GH4098 is a Waspaloy alloy used in Aircraft afterburner components, Combustion chamber liners, Thermal protection panels. It offers 1000°C intermittent service and Sheet metal fabricable.

What is the chemical composition of GH4098?

GH4098 is a controlled-composition Waspaloy alloy supplied to GB/T 14994. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is GH4098 available in?

GH4098 is regularly supplied in Forging, Wire, Bar & Rod, Plate & Sheet, Strip. Custom forms and dimensions available on request.

What is the maximum service temperature of GH4098?

GH4098 is rated for service up to 1000°C. Contact our metallurgy team for specific application recommendations.

Need GH4098 material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google