Reference table

AMS specifications by product form

13 AMS documents across the stocked grades, grouped by the product form written into each SAE spec title: filter to your form and get the governing number, with the four 718-family specs linking to dedicated pages.

Grade AMS spec Product form (per SAE title) Site page
Inconel 718 AMS 5662 Bar, forgings spec page →
Inconel 718 AMS 5663 Bar, forgings spec page →
Inconel 625 AMS 5666 Other ,
Hastelloy X AMS 5536 Sheet, strip ,
Hastelloy X AMS 5754 Bar, forgings ,
Nimonic 80A AMS 5763 Bar, forgings ,
Waspaloy AMS 5708 Bar, forgings ,
Waspaloy AMS 5709 Bar, forgings ,
Waspaloy AMS 5544 Plate, sheet, strip ,
MP35N AMS 5844 Bar, wire ,
MP35N AMS 5845 Bar, wire ,
L605 AMS 5759 Bar, forgings ,
L605 AMS 5537 Sheet, strip ,

Frequently Asked Questions (FAQ)

Why does the form column matter so much for AMS numbers?

Because AMS documents are product-form specific: the melt practice, condition and test regime are written for the product shape in the title. A bar ordered to AMS 5662 and plate ordered to AMS 5596 describe the same Inconel 718 chemistry through different acceptance windows, the form decides which number belongs on the drawing.

Why is one AMS number missing from this table?

The 1J22 soft-magnetic grade lists "AMS 7717 equivalent" in its verified standards, an equivalence note, not an SAE document citation, so it does not belong in a lookup of actual AMS specifications. It stays on the governing-standards table where the distinction is labelled.

Where do the deep spec pages live?

Four Inconel 718 AMS documents have dedicated pages on this site, AMS 5662 and 5663 bar, AMS 5596 plate and AMS 5597 sheet, each with the verified condition, mechanical anchors and a direct link to the SAE record. 2 of the 13 table rows link straight through.

Quoting against an AMS number?

Send the spec, the form and the sizes, we confirm the melt practice and condition the spec requires and quote with full heat traceability.