Incoloy Series
Nickel Alloys

Incoloy Series

Fe-Ni-Cr alloys balancing high-temperature strength with lower alloy cost, plus age-hardenable grades for sour-gas and fastener duty.

About Incoloy Series

Incoloy Series is a series of nickel-base alloys. Fe-Ni-Cr alloys balancing high-temperature strength with lower alloy cost, plus age-hardenable grades for sour-gas and fastener duty. The series currently covers 6 grades, supplied as Forging, Wire, Spring Wire, Flange, Bar & Rod, Plate & Sheet, Strip, Pipe & Tube to ASTM B409, ASTM B407, ASTM B163, ASTM B408 requirements. Orders ship with 100% heat-traceable mill test certification, and technical enquiries receive a substantive reply within 24 hours.

Where This Series Fits

  • High iron content delivers high-temperature strength and oxidation resistance at a significantly lower cost than nickel-base grades
  • Incoloy 800 / 800H / 800HT are one composition family supplied in different heat-treatment and grain-size conditions
  • Incoloy 825 adds molybdenum and copper for mixed-acid duty such as sulphuric-acid coolers and phosphoric-acid evaporators
  • Incoloy 925 and A-286 are age-hardenable, targeting sour-gas wellhead components and high-temperature fasteners respectively

Available Forms

ForgingWireSpring WireFlangeBar & RodPlate & SheetStripPipe & Tube

Applicable Standards

ASTM B409ASTM B407ASTM B163ASTM B408

Incoloy Series: Grade Comparison

6 grades
Grade Max service temp Density Typical use
Incoloy 800 1100 °C 7.94 g/cm³ Ni-Fe-Cr alloy for high-temperature heat exchangers and process piping in petrochemical plants.
Incoloy 800H 1100 °C 7.94 g/cm³ Solution-annealed Incoloy 800 with enhanced high-temperature creep strength.
Incoloy 800HT 1100 °C 7.94 g/cm³ Fine-grain variant of 800H with optimized high-temperature ductility for forming operations.
Incoloy 825 540 °C 8.14 g/cm³ Ni-Fe-Cr-Mo-Cu alloy with exceptional resistance to sulfuric and phosphoric acid corrosion.
Incoloy 925 650 °C 8.14 g/cm³ Age-hardenable Incoloy for high-strength sour gas wellhead and downhole equipment.
Incoloy A-286 700 °C 7.94 g/cm³ Fe-Ni-Cr precipitation-hardenable alloy for high-temperature fasteners and automotive turbocharger springs.
How to request a quote — send grade, form, dimensions, standard and quantity; we reply within 24 hours →

Frequently Asked Questions (FAQ)

What is the Incoloy Series?

Incoloy Series is a series of nickel-base alloys. Fe-Ni-Cr alloys balancing high-temperature strength with lower alloy cost, plus age-hardenable grades for sour-gas and fastener duty. RAS Thermal supplies 6 grades in this series.

What standards apply to Incoloy Series materials?

Supply follows ASTM B409, ASTM B407, ASTM B163, ASTM B408, with the mill test certificate referencing the exact designation called out on your purchase order.

How do I request a quote for Incoloy grades?

Send the grade, form, dimensions, standard and quantity, our metallurgy team replies within 24 hours with availability, pricing and a sample mill test certificate on request.

Need a specific Incoloy grade?

Send your specification with grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google