1J22
HiperCo 50 equivalent: the Fe-Co-V alloy with the highest saturation induction of any soft magnetic material.
Introduction
§01, GeneralNeed maximum flux in minimum volume? 1J22 (HiperCo 50 equivalent) hits 2.4 T saturation induction, the highest of any commercial soft magnetic material. That's why solenoid armatures, pole pieces and magnetic bearing components in aerospace and defense keep specifying an iron-cobalt-vanadium alloy that carries more flux per gram than anything else on the shelf.
Quick Facts
- Density
- 8.2 g/cm³
- Max Service Temp
- 450°C
- Series
- Precision
Chemical Composition
GB/T 15018, 1J22 (Fe-Co-V), nominal wt%
| Element | Symbol | Content (wt%) | Role |
|---|---|---|---|
| Cobalt | Co | 48.0 – 51.0 | High saturation magnetization |
| Vanadium | V | 1.4 – 1.8 | Ductility & aging control |
| Carbon | C | 0.04 max | Controlled residual |
| Iron | Fe | Balance | Base |
Mechanical & Physical Properties
Manufacturer datasheet, typical (soft magnetic alloy — mechanicals vary with heat treat)
| Property | Value | Condition |
|---|---|---|
| Tensile Strength (annealed) | ≈500–700 MPa | Typical, annealed |
| Saturation Flux Density | ≈2.35 T | Key design property |
| Curie Temperature | ≈940 °C | Physical |
| Density | 8.2 g/cm³ | Physical |
Applicable Standards & Product Forms
1J22 · UNS — · GB/T 1J22
| Standard | Product Form |
|---|---|
| GB/T 15018 | Cold-rolled strip / bar |
Available Product Forms
§02, FormsKey Characteristics
§03, FeaturesTypical Uses
§04, ApplicationsExplore Related Alloys
More Precision Grades
Rated 450°C, in the same class as this grade, also used for electromagnetic, same Precision series.
Rated 350°C, lower than this grade, also used for precision, same Precision series.
Rated 450°C, in the same class as this grade, same Precision series.
Rated 230°C, lower than this grade, also used for precision, same Precision series.
Pricing
How 1J22 is priced
We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.
This grade specifies nickel as balance rather than as a minimum, so there is no single published figure to anchor the metal content. The price still builds the same way: the alloy charge at index prices, then melting, rolling or forging, heat treatment, testing and yield loss.
Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.
What moves the number
- Metal content
- Ni · Mo · Nb · Cr, at their index prices
- Product form
- Plate to seamless pipe is the widest step
- Size & tolerance
- Process hours, not alloy price
- Melting route
- Air / ESR / VAR
- Test scope
- UT, PMI, hardness, third-party witness
Frequently Asked Questions
1J22 FAQWhat is 1J22 used for?
1J22 is a Precision alloy used in Aerospace solenoid armatures, Magnetic bearing pole pieces, High-flux generator rotors. It offers Highest saturation induction (2.4 T) and HiperCo 50 equivalent.
What is the chemical composition of 1J22?
1J22 is a controlled-composition Precision alloy supplied to GB/T 14986 and AMS 7717 equivalent. We provide the full mill test certificate with heat-specific chemistry on request.
What forms is 1J22 available in?
1J22 is regularly supplied in Wire, Strip, Plate & Sheet, Bar & Rod. Custom forms and dimensions available on request.
What is the maximum service temperature of 1J22?
1J22 is rated for service up to 450°C. Contact our metallurgy team for specific application recommendations.
Need 1J22 material?
Request a quote with your specification: grade, form, dimensions and quantity.