4J29 alloy products
Material Family / Precision

4J29

Kovar: the Fe-Ni-Co expansion alloy for glass-to-metal and ceramic-to-metal seals in electronics packaging.

Introduction

§01, General

Seal glass to metal and the joint lives or dies on expansion match. 4J29 (Kovar) tracks borosilicate glass and alumina ceramics closely through the thermal cycle, so the hermetic seal holds. Electronic packages, transistor headers, microwave tubes and optoelectronic housings have made it the default sealing alloy for decades.

ASTM F15GB/T 14986MIL-I-23011

Quick Facts

Density
8.17 g/cm³
Max Service Temp
450°C
Series
Precision

Chemical Composition

GB/T 15018 / ASTM F15 (Kovar), nominal wt%

Element Symbol Content (wt%) Role
Nickel Ni 28.5 – 29.5 Expansion match to glass
Cobalt Co 16.8 – 17.8 Expansion curve control
Manganese Mn 0.4 max Deoxidiser
Silicon Si 0.3 max Controlled residual
Carbon C 0.05 max Controlled residual
Iron Fe Balance Base

Mechanical & Physical Properties

Manufacturer datasheet, typical

Property Value Condition
Tensile Strength (annealed) ≈480–550 MPa Typical, annealed
CTE (20–400 °C) ≈5.9×10⁻⁶ /K Key sealing property
Density 8.17 g/cm³ Physical

Applicable Standards & Product Forms

4J29 · UNS K94610 · GB/T 4J29

Standard Product Form
ASTM F15 Sheet / rod / wire (glass sealing)
GB/T 15018 Strip / bar / wire
WireStripBar & RodPlate & Sheet

Available Product Forms

§02, Forms
WireStripBar & RodPlate & Sheet

Key Characteristics

§03, Features
Thermal expansion matches borosilicate glass
Kovar / ASTM F15 standard
Hermetic seal qualified
Good plating and brazing
Leak-tight to 10⁻⁹ cc He/s

Typical Uses

§04, Applications
Transistor and IC hermetic packages
Microwave tube windows
Optoelectronic device housings
Reed switch glass seals
Cryogenic electrical feedthroughs

Pricing

How 4J29 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

What can be stated precisely is the nickel floor: at 28.5% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of 4J29 is about USD 4.36. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

4J29 FAQ

What is 4J29 used for?

4J29 is a Precision alloy used in Transistor and IC hermetic packages, Microwave tube windows, Optoelectronic device housings. It offers Thermal expansion matches borosilicate glass and Kovar / ASTM F15 standard.

What is the chemical composition of 4J29?

4J29 is a controlled-composition Precision alloy supplied to ASTM F15 and GB/T 14986. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is 4J29 available in?

4J29 is regularly supplied in Wire, Strip, Bar & Rod, Plate & Sheet. Custom forms and dimensions available on request.

What is the maximum service temperature of 4J29?

4J29 is rated for service up to 450°C. Contact our metallurgy team for specific application recommendations.

Need 4J29 material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google