L605 alloy products
Material Family / Cobalt-Based

L605

Co-Cr-W-Ni alloy for aerospace bearing components and high-temperature wear applications.

Introduction

§01, General

Galling and fretting lose battles before heat does. L605 (Haynes 25) is a cobalt-chromium-tungsten-nickel alloy with high-temperature strength plus oxidation resistance to 980°C, and the cobalt base naturally resists wear. Bearing races, wear rings and combustion hardware: dense at 9.13 g/cm³, tough, and hard to replace.

Cross-Reference

UNS: UNS R30605
GB/T: GB GH605
Series: Cobalt-Based
Density: 9.13 g/cm³
Max Temp: 980°C
Standards: AMS 5759 · AMS 5537 · ASTM F90

Quick Facts

UNS
R30605
GB
GH605
Density
9.13 g/cm³
Max Service Temp
980°C
Series
Cobalt-Based

Chemical Composition

AMS 5759 / ASTM F90 (R30605, Haynes 25), wt%

Element Symbol Content (wt%) Role
Cobalt Co Balance Base; hot strength
Chromium Cr 19.0 – 21.0 Oxidation & sulfidation resistance
Tungsten W 14.0 – 16.0 Solid-solution strengthening
Nickel Ni 9.0 – 11.0 Phase stability
Iron Fe 3.0 max Controlled residual
Carbon C 0.05 – 0.15 Carbide strengthening
Manganese Mn 1.0 – 2.0 Deoxidiser

Mechanical & Physical Properties

Manufacturer datasheet, typical (annealed)

Property Value Condition
Tensile Strength 895 MPa Typical, annealed RT
Yield Strength (0.2% offset) 470 MPa Typical, annealed RT
Elongation 45% Typical, annealed RT
Density 9.13 g/cm³ Physical

Applicable Standards & Product Forms

L605 · UNS R30605 · GB/T GH605

Standard Product Form
AMS 5759 Bar & forgings
AMS 5537 Sheet & strip
ASTM F90 Medical-grade wire
ForgingWireBar & Rod

Available Product Forms

§02, Forms
ForgingWireBar & Rod

Key Characteristics

§03, Features
Excellent wear and galling resistance
Oxidation resistant to 980°C
Non-magnetic
Biocompatible (ASTM F90)
Aerospace bearing standard

Typical Uses

§04, Applications
Aerospace bearing races and rings
Gas turbine wear components
Combustion chamber hardware
Prosthetic medical devices
High-temperature fasteners

Pricing

How L605 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

What can be stated precisely is the nickel floor: at 9% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of L605 is about USD 1.38. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

L605 FAQ

What is L605 used for?

L605 is a Cobalt-Based alloy used in Aerospace bearing races and rings, Gas turbine wear components, Combustion chamber hardware. It offers Excellent wear and galling resistance and Oxidation resistant to 980°C.

What is the chemical composition of L605?

L605 is a controlled-composition Cobalt-Based alloy supplied to AMS 5759 and AMS 5537. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is L605 available in?

L605 is regularly supplied in Forging, Wire, Bar & Rod. Custom forms and dimensions available on request.

What is the maximum service temperature of L605?

L605 is rated for service up to 980°C. Contact our metallurgy team for specific application recommendations.

Need L605 material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google