MP35N alloy products
Material Family / Cobalt-Based

MP35N

Co-Ni-Cr-Mo alloy with ultra-high tensile strength, fatigue endurance and biocompatibility.

Introduction

§01, General

Severe cold work pushes MP35N past what most superalloys reach, and it stays non-magnetic the whole way. Ultra-high tensile strength, exceptional fatigue life, corrosion resistance and biocompatibility in one Co-Ni-Cr-Mo chemistry: that's the resume behind medical implants, aerospace fasteners and MRI-compatible springs. Density 8.43 g/cm³, service to 425°C.

Cross-Reference

UNS: UNS R30035
Series: Cobalt-Based
Density: 8.43 g/cm³
Max Temp: 425°C
Standards: ASTM F562 · AMS 5844 · AMS 5845 · ISO 5832-6

Quick Facts

UNS
R30035
Density
8.43 g/cm³
Max Service Temp
425°C
Series
Cobalt-Based

Chemical Composition

ASTM F562 / AMS 5844 (R30035), wt%

Element Symbol Content (wt%) Role
Nickel Ni 33.0 – 37.0 Multiphase matrix
Cobalt Co 33.0 – 37.0 Multiphase strengthening
Chromium Cr 19.0 – 21.0 Corrosion & biocompatibility
Molybdenum Mo 9.0 – 10.5 Strengthening
Titanium Ti 1.0 max Controlled residual
Iron Fe 1.0 max Controlled residual
Carbon C 0.03 max Controlled residual

Mechanical & Physical Properties

AMS 5844, typical (aged)

Property Value Condition
Tensile Strength 1275 MPa min Typical, aged RT (higher when cold-worked + aged)
Yield Strength (0.2% offset) 830 MPa min Typical, aged RT
Elongation 12% min Typical, aged RT
Density 8.43 g/cm³ Physical

Applicable Standards & Product Forms

MP35N · UNS R30035 · GB/T —

Standard Product Form
ASTM F562 Medical bar & wire
AMS 5844 Bar (aged)
AMS 5845 Wire
ISO 5832-6 Implant grade
ForgingWireSpring WireBar & RodStrip

Available Product Forms

§02, Forms
ForgingWireSpring WireBar & RodStrip

Key Characteristics

§03, Features
Ultra-high tensile strength (>1800 MPa achievable)
Non-magnetic (MRI compatible)
Excellent fatigue life
Biocompatible per ASTM F562
Seawater corrosion resistant

Typical Uses

§04, Applications
Medical implants and guidewires
Aerospace fasteners
High-performance springs
Downhole tool components
Orthopedic devices

Pricing

How MP35N is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

What can be stated precisely is the nickel floor: at 33% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of MP35N is about USD 5.05. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

MP35N FAQ

What is MP35N used for?

MP35N is a Cobalt-Based alloy used in Medical implants and guidewires, Aerospace fasteners, High-performance springs. It offers Ultra-high tensile strength (>1800 MPa achievable) and Non-magnetic (MRI compatible).

What is the chemical composition of MP35N?

MP35N is a controlled-composition Cobalt-Based alloy supplied to ASTM F562 and AMS 5844. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is MP35N available in?

MP35N is regularly supplied in Forging, Wire, Spring Wire, Bar & Rod, Strip. Custom forms and dimensions available on request.

What is the maximum service temperature of MP35N?

MP35N is rated for service up to 425°C. Contact our metallurgy team for specific application recommendations.

Need MP35N material?

Request a quote with your specification: grade, form, dimensions and quantity.

Request a Quote
Add RAS Thermal as a preferred source on Google