Monel K-500

Age-hardened nickel-copper alloy combining corrosion resistance with high strength.

Introduction

§01, General

Take Monel 400's seawater corrosion resistance, add aluminum and titanium, age it, and you get 965 MPa tensile with 690 MPa yield. K-500 is what you spec when marine hardware also has to be strong: propeller shafts, pump shafts, valve trim in seawater and sour gas. It stays non-magnetic down to -100°C.

Cross-Reference

UNS: UNS N05500
Series: Monel
Density: 8.44 g/cm³
Max Temp: 315°C
Standards: ASTM B865 · ASTM B164 · AMS 4676 · UNS N05500

Quick Facts

UNS
N05500
Density
8.44 g/cm³
Max Service Temp
315°C
Series
Monel

Chemical Composition

ASTM B865 / AMS 4676 (N05500), wt%

Element Symbol Content (wt%) Role
Nickel Ni 63.0 min Base matrix
Copper Cu 27.0 – 33.0 Seawater & acid resistance
Aluminum Al 2.3 – 3.15 γ′ age hardening
Titanium Ti 0.35 – 0.85 γ′ age hardening
Iron Fe 2.0 max Controlled residual
Manganese Mn 1.5 max Deoxidiser
Carbon C 0.25 max Controlled residual

Mechanical & Physical Properties

Manufacturer datasheet, typical (aged)

Property Value Condition
Tensile Strength 1100 MPa Typical, aged bar RT
Yield Strength (0.2% offset) 760 MPa Typical, aged bar RT
Elongation 20% Typical, aged bar RT
Density 8.44 g/cm³ Physical
Melting Range 1315–1350 °C Physical

Applicable Standards & Product Forms

Monel K-500 · UNS N05500 · GB/T —

Standard Product Form
ASTM B865 Bar & Rod (aged)
ASTM B164 Rod & Bar (base)
AMS 4676 Bar & rod (aerospace aged)
UNS N05500 Cross-reference designation
ForgingWireSpring WireBarRodStrip

Available Product Forms

§02, Forms
ForgingWireSpring WireBarRodStrip

Key Characteristics

§03, Features
Age-hardened for high strength
Seawater and sour-gas corrosion resistant
Non-magnetic up to -100°C
AMS 4676 certified

Typical Uses

§04, Applications
Marine propeller shafts and bearings
Oil-well drill collars and tools
Pump and valve trim in seawater
High-strength fasteners and springs
Chemical processing agitators

Chemical Composition

ElementMin %Max %Typical %
Ni63.070.066.0
Cu27.033.029.5
Al2.303.152.75
Ti0.350.850.60
Fe-2.01.0
Mn-1.50.8
C-0.250.10
S-0.010.005

Mechanical Properties

TemperatureUTSYieldElongationHardness
Room965 MPa690 MPa20%27 HRC
200°C905 MPa650 MPa22%-
315°C830 MPa590 MPa24%-

Physical Properties

PropertyValueNote
Density8.44 g/cm³at 20°C
Melting range1315 - 1350°Csolidus-liquidus
Thermal expansion13.7 μm/m·K20-100°C
Thermal conductivity17.5 W/m·Kat 20°C
Specific heat419 J/kg·Kat 20°C

Industries

Marine, Oil & Gas, Chemical Processing, Power Generation.

Pricing

How Monel K-500 is priced

We do not publish a per-kilogram band. The alloy charge re-prices with nickel and molybdenum, and the rest of the number depends on form, size, melting route and test scope — a figure printed here would be stale before it shipped.

What can be stated precisely is the nickel floor: at 63% nickel (specification minimum) and an LME nickel cash price of USD 15,310/t on 2026-11-20, the nickel content of one kilogram of Monel K-500 is about USD 9.65. Everything above that is conversion: melting, rolling or forging, heat treatment, testing and yield loss.

Nickel reference: LME official cash settlement via Westmetall, 2026-11-20. Verify the current figure.

What moves the number

Metal content
Ni · Mo · Nb · Cr, at their index prices
Product form
Plate to seamless pipe is the widest step
Size & tolerance
Process hours, not alloy price
Melting route
Air / ESR / VAR
Test scope
UT, PMI, hardness, third-party witness
Send form & quantity for a price

Frequently Asked Questions

Monel K-500 FAQ

What is Monel K-500 used for?

Monel K-500 is a Monel alloy used in Marine propeller shafts and bearings, Oil-well drill collars and tools, Pump and valve trim in seawater. It offers Age-hardened for high strength and Seawater and sour-gas corrosion resistant.

What is the chemical composition of Monel K-500?

Monel K-500 is a controlled-composition Monel alloy supplied to ASTM B865 and ASTM B164. We provide the full mill test certificate with heat-specific chemistry on request.

What forms is Monel K-500 available in?

Monel K-500 is regularly supplied in Forging, Wire, Spring Wire, Bar, Rod, Strip. Custom forms and dimensions available on request.

What is the maximum service temperature of Monel K-500?

Monel K-500 is rated for service up to 315°C. Contact our metallurgy team for specific application recommendations.