A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
As strength anchors from the verified feature sets, MP35N achieves over 1800 MPa tensile while staying non-magnetic per ASTM F562, and Nimonic 80A carries gamma-prime strengthening with service to 815 °C.
What this page covers
Nuclear reactor internals demand documented, stable materials. At RAS Thermal the nuclear grades are Inconel 625 (nuclear reactor components, verified pitting and crevice resistance), Inconel 718 (fasteners and structural hardware) and Hastelloy X (high-temperature internals and ducting).
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Reactor internals: 625. Fasteners: 718. High-temp ducting: Hastelloy X. Traceability: heat + EN 10204.
What this means for your selection
Nuclear reactor internals demand documented, stable materials. At RAS Thermal the nuclear grades are Inconel 625 (nuclear reactor components, verified pitting and crevice resistance), Inconel 718 (fasteners and structural hardware) and Hastelloy X (high-temperature internals and ducting). The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Run the list top to bottom before the enquiry goes out, that is what keeps the part inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- Inconel 718: 8.19 g/cm³ · 650 °C, and typical use: rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
- Inconel 625: 8.44 g/cm³ · 980 °C, and typical use: seawater piping, chemical processing and subsea connectors where weldability and corrosion resistance decide.
- Hastelloy C-276: 8.89 g/cm³ · 400 °C, and typical use: chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.
- Hastelloy X: 8.22 g/cm³ · 1100 °C, and typical use: gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C.
- Monel 400: 8.8 g/cm³ · 540 °C, and typical use: seawater piping, HF acid alkylation units and marine shafts.
- Nimonic 80A: 8.19 g/cm³ · 815 °C, and typical use: exhaust valves, turbine blades and high-temperature springs to 815 °C.
- Waspaloy: 8.22 g/cm³ · 870 °C, and typical use: turbine discs, rings, shafts and high-temperature fasteners.
- Nickel 200: 8.89 g/cm³ · 315 °C, and typical use: caustic soda evaporator tubes, spinnerets and electrical terminals.
- Incoloy 800: 7.94 g/cm³ · 1100 °C, and typical use: petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.
- Incoloy 800H: 7.94 g/cm³ · 1100 °C, and typical use: ASME pressure vessels, steam methane reformers and power plant superheaters.
- Incoloy 800HT: 7.94 g/cm³ · 1100 °C, and typical use: hot-formed pressure vessel heads, tube sheets and reformer tubes.
- Incoloy 825: 8.14 g/cm³ · 540 °C, and typical use: sulfuric acid coolers, phosphoric acid evaporators and offshore production piping.
- Incoloy 925: 8.14 g/cm³ · 650 °C, and typical use: sour gas wellhead components, downhole completion tools and high-strength fasteners.
Related resources
Each link below takes one grade or one sub-topic and carries the same verified numbers with it.
- certification, Inconel 718
- certification, Inconel 625
- certification, Hastelloy C-276
- certification, Hastelloy X
- certification, Monel 400
- certification, Nimonic 80A
- certification, Waspaloy
- certification, Nickel 200
- certification, Incoloy 800
- certification, Incoloy 800H
- certification, Incoloy 800HT
- certification, Incoloy 825
- certification, Incoloy 925