Selection guide
Corrosion Resistant Alloys: Nine Nickel Grades by Media
Nine nickel grades grouped by medium: Ni-Cr-Mo for mixed oxidising and reducing service, Ni-Mo for reducing acids, Ni-Cu for seawater and HF.
TL;DR The corrosion resistant alloys here split by medium, not by strength. Ni-Cr-Mo grades (Hastelloy C-276, C22, C-4) cover mixed oxidising and reducing service; Ni-Mo grades (B-2, B-3) are for reducing acids; Monel 400 is the Ni-Cu answer for seawater and hydrofluoric acid; and Inconel 600, 625 and Incoloy 800HT carry oxidation resistance at temperature rather than immersion resistance.
What it is Corrosion resistant alloys are chosen by the medium first: what oxidises, what reduces, what…
Corrosion resistant alloys are chosen by the medium first: what oxidises, what reduces, what contains chlorides, and at what temperature. This page groups the nine nickel grades stocked by RAS Thermal along those lines, with the UNS number and the ceiling for each, so the shortlist forms before the datasheet opens.
Mixed oxidising + reducing
C-276 · C22 · C-4
Reducing acids (Ni-Mo)
B-2 · B-3
Seawater and HF
Monel 400
Oxidation at temperature
600 · 625 · 800HT
Grades on this page
9
Related Products & Resources
Hastelloy C-276 (N10276) — the default for mixed aggressive mediaHastelloy C22 (N06022) — strongest on oxidising mediaHastelloy C-4 (N06455) — stable, no intergranular precipitationHastelloy B-2 (N10665) — Ni-Mo for reducing serviceHastelloy B-3 (N10675) — third-generation Ni-Mo, better fabricabilityInconel 625 (N06625) — corrosion resistance plus strength to 980 °CInconel 600 (N06600) — oxidation resistance to 1095 °CIncoloy 800HT (N08811) — high-temperature ductility to 1100 °CMonel 400 (N04400) — seawater and hydrofluoric acid serviceChemical processing: which grade for which vesselMarine and offshore service
Specifying a corrosion resistant alloy?
Send the medium, the concentration, the service temperature and the form you need. We reply with a shortlist from the nine grades above, plus the standards each one is supplied against.