A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.
What this page covers
Power generation pushes superalloys toward their temperature ceilings. At RAS Thermal the generation grades are Hastelloy X (combustion chambers, oxidation to 1100 °C), Inconel 625 (oxidation resistant to 980 °C), Waspaloy (turbine hardware to 870 °C) and Inconel 718 (fasteners and discs).
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Combustion: Hastelloy X (1100 °C). Heat exchanger: 625. Turbine: Waspaloy · 718. Furnace hardware: X · GH3044.
What this means for your selection
Power generation pushes superalloys toward their temperature ceilings. At RAS Thermal the generation grades are Hastelloy X (combustion chambers, oxidation to 1100 °C), Inconel 625 (oxidation resistant to 980 °C), Waspaloy (turbine hardware to 870 °C) and Inconel 718 (fasteners and discs). The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- Inconel 718: 8.19 g/cm³ · 650 °C, and typical use: rotating hardware, high-strength fasteners and subsea wellhead components from cryogenic to 650 °C.
- Inconel 625: 8.44 g/cm³ · 980 °C, and typical use: seawater piping, chemical processing and subsea connectors where weldability and corrosion resistance decide.
- Hastelloy C-276: 8.89 g/cm³ · 400 °C, and typical use: chemical reactor internals, FGD scrubbers and sour-gas piping where pitting and stress-corrosion cracking are the enemy.
- Hastelloy X: 8.22 g/cm³ · 1100 °C, and typical use: gas turbine combustion chambers, afterburners and furnace hardware above 1000 °C.
- Monel 400: 8.8 g/cm³ · 540 °C, and typical use: seawater piping, HF acid alkylation units and marine shafts.
- Nimonic 80A: 8.19 g/cm³ · 815 °C, and typical use: exhaust valves, turbine blades and high-temperature springs to 815 °C.
- Waspaloy: 8.22 g/cm³ · 870 °C, and typical use: turbine discs, rings, shafts and high-temperature fasteners.
- Nickel 200: 8.89 g/cm³ · 315 °C, and typical use: caustic soda evaporator tubes, spinnerets and electrical terminals.
- Incoloy 800: 7.94 g/cm³ · 1100 °C, and typical use: petrochemical furnace tubes, heat exchanger bundles and process piping from 600 to 1100 °C.
- Incoloy 800H: 7.94 g/cm³ · 1100 °C, and typical use: ASME pressure vessels, steam methane reformers and power plant superheaters.
- Incoloy 800HT: 7.94 g/cm³ · 1100 °C, and typical use: hot-formed pressure vessel heads, tube sheets and reformer tubes.
- Incoloy 825: 8.14 g/cm³ · 540 °C, and typical use: sulfuric acid coolers, phosphoric acid evaporators and offshore production piping.
- Incoloy 925: 8.14 g/cm³ · 650 °C, and typical use: sour gas wellhead components, downhole completion tools and high-strength fasteners.
Related resources
Follow the links for the per-grade pages, the figures there match the ones on this page.
- service temperature, Inconel 718
- service temperature, Inconel 625
- service temperature, Hastelloy C-276
- service temperature, Hastelloy X
- service temperature, Monel 400
- service temperature, Nimonic 80A
- service temperature, Waspaloy
- service temperature, Nickel 200
- service temperature, Incoloy 800
- service temperature, Incoloy 800H
- service temperature, Incoloy 800HT
- service temperature, Incoloy 825
- service temperature, Incoloy 925