A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
As a chemistry anchor from the verified composition tables, Inconel 718 spans Ni 50.0-55.0%, Cr 17.0-21.0%, Mo 2.80-3.30% and Nb 4.75-5.50%, and Hastelloy C-276 spans Mo 15.0-17.0%, Cr 14.5-16.5%, Fe 4.0-7.0% and W 3.0-4.5%.
What this page covers
A superalloy order is only actionable through its standard, and the form decides the document. At RAS Thermal the ASTM map runs: B637 for precipitation-hardened bar and forgings (Inconel 718, the Nimonic ladder, Waspaloy), B443 for Inconel 625 flat product, B168 for the Inconel 600/601/690 flat family, B575 for the Hastelloy C line, B435 for Hastelloy X sheet and plate, B163 and B407 for incoloy seamless tube, B408 and B164 and B160 for bar and rod, with the F-series (F562, F90, F15, F1684) covering the cobalt and precision grades. Cite the standard and the UNS together so the certificate matches the drawing.
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Bar & forgings: B637 (7 grades) · B408 · B164 · B160. Flat product: B443 · B168 · B575 · B435. Seamless tube: B163 (4 incoloy grades) · B407 (800 family). Precision & cobalt: F562 · F90 · F15 · F1684.
What this means for your selection
A superalloy order is only actionable through its standard, and the form decides the document. At RAS Thermal the ASTM map runs: B637 for precipitation-hardened bar and forgings (Inconel 718, the Nimonic ladder, Waspaloy), B443 for Inconel 625 flat product, B168 for the Inconel 600/601/690 flat family, B575 for the Hastelloy C line, B435 for Hastelloy X sheet and plate, B163 and B407 for incoloy seamless tube, B408 and B164 and B160 for bar and rod, with the F-series (F562, F90, F15, F1684) covering the cobalt and precision grades. Cite the standard and the UNS together so the certificate matches the drawing. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Five checks, in order. Each one keeps the component inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- ASTM B637: Inconel 718 · X-750 · Nimonic 75/80A/90/901 · Waspaloy, and typical use: Bar & forgings.
- ASTM B443: Inconel 625, and typical use: Plate, sheet & strip.
- ASTM B168: Inconel 600 · 601 · 690, and typical use: Plate, sheet & strip.
- ASTM B575: Hastelloy C · C-4 · C-22 · C-276, and typical use: Plate, sheet & strip.
- ASTM B435: Hastelloy X · GH3044, and typical use: Plate, sheet & strip.
- ASTM B163: Incoloy 800 · 800H · 800HT · 825, and typical use: Seamless pipe & tube.
- ASTM B407: Incoloy 800 · 800H · 800HT, and typical use: Seamless pipe & tube.
- ASTM B408: Incoloy 800, and typical use: Rod & bar.
- ASTM B164: Monel 400 · K-500, and typical use: Rod, bar & wire.
- ASTM B160: Nickel 200, and typical use: Rod & bar.
Related resources
The pages below drill into this topic and document the same verified numbers.
- ASTM B637, bar & forgings
- ASTM B443, Inconel 625 plate
- ASTM B168, Inconel 600/601/690 plate
- ASTM B575, Hastelloy C family plate
- ASTM B435, Hastelloy X plate
- ASTM B163, incoloy seamless tube
- ASTM B407, 800-family pipe & tube
- ASTM B408, Incoloy 800 bar
- ASTM B164, Monel bar & wire
- ASTM B160, Nickel 200 bar
- AMS 5662, Inconel 718 bar (aerospace)
- AMS 5596, Inconel 718 sheet, strip & plate
- Inconel 718 equivalent grades
- Hastelloy C-276 equivalent standards
- AMS specification lookup by form
- Governing standards by alloy