A superalloy is an alloy engineered for sustained service at high temperature or in aggressive media, and every figure on this page traces back to a verified datasheet or governing standard.
For reference, the verified room-temperature elongation figures are Inconel 718 at 12%, Hastelloy C-276 at 40% and Monel K-500 at 20%. Elongation tracks the heat-treatment condition, so the mill certificate states the value for your heat.
What this page covers
The product form is the second decision after the grade. At RAS Thermal the verified ranges are: bar and rod Ø6-350 mm · length to 6,000 mm, and plate and sheet Thk. 0.5-80 mm · width to 2,000 mm, and strip Thk. 0.05-3.0 mm · width 4-600 mm, and pipe and tube OD 6-219 mm · wall 0.5-20 mm, and wire Ø0.10-12.0 mm in coil, spool or cut-to-length, and plus forgings Ring-rolled, upset and open-die from 5 kg to 3,000 kg and flanges to ASME B16.5 / B16.47. The form follows the machined part.
The verified numbers
Every figure on this page is drawn from our verified superalloy datasheets and the governing standards (ASTM B637/B443/B575/B164/B160, AMS, GB/T 14986). Bar & Rod: Ø6-350 mm · length to 6,000 mm. Plate & Sheet: Thk. 0.5-80 mm · width to 2,000 mm. Strip: Thk. 0.05-3.0 mm · width 4-600 mm. Pipe & Tube: OD 6-219 mm · wall 0.5-20 mm.
What this means for your selection
The product form is the second decision after the grade. At RAS Thermal the verified ranges are: bar and rod Ø6-350 mm · length to 6,000 mm, and plate and sheet Thk. 0.5-80 mm · width to 2,000 mm, and strip Thk. 0.05-3.0 mm · width 4-600 mm, and pipe and tube OD 6-219 mm · wall 0.5-20 mm, and wire Ø0.10-12.0 mm in coil, spool or cut-to-length, and plus forgings Ring-rolled, upset and open-die from 5 kg to 3,000 kg and flanges to ASME B16.5 / B16.47. The form follows the machined part. The table below takes each grade’s temperature ceiling, best duty and available form, and the related pages carry the same verified numbers one level deeper. Decision first, then the data behind it.
How to select the right option for your process
Work through these checks in order so the component stays inside its specification:
- Step 1: Confirm the maximum service temperature. Fix the peak continuous service temperature the component will see. It decides whether a precipitation-hardened grade such as Inconel 718 (650 °C) or an oxidation-resistant solid-solution grade such as Hastelloy X (1100 °C) is in the running.
- Step 2: Match the environment and alloy family. Identify the corroding or oxidizing media and match the family: Ni-Cr-Mo for wet corrosion, Ni-Cu for seawater and hydrofluoric acid, cobalt-base for wear and biocompatibility, precision grades for controlled physical properties.
- Step 3: Choose the product form. Select the semi-finished form: bar and rod, plate and sheet, strip, pipe and tube, wire, or a forged ring, disc or shaft, against the machined part and quantity.
- Step 4: Set the dimensions and tolerances. State the finished dimensions, condition (hot rolled, cold drawn, solution annealed, spring temper) and surface finish against the form’s stock range.
- Step 5: State the standard and certificate. Declare the governing ASTM / AMS / GB-T standard and the certification level, EN 10204 3.1 with heat-specific chemistry, or 3.2 third-party witnessed.
How the candidate options compare
- Bar & Rod: Ø6-350 mm · length to 6,000 mm, and typical use: Machined valve trim, fasteners, pump shafts, downhole tools.
- Plate & Sheet: Thk. 0.5-80 mm · width to 2,000 mm, and typical use: Pressure vessels, heat exchangers, reactor internals.
- Strip: Thk. 0.05-3.0 mm · width 4-600 mm, and typical use: Bellows, diaphragms, magnetic cores, sealing rings.
- Pipe & Tube: OD 6-219 mm · wall 0.5-20 mm, and typical use: Umbilical lines, condenser tubing, chemical piping.
- Wire: Ø0.10-12.0 mm in coil, spool or cut-to-length, and typical use: Springs, fasteners, welding consumables, sensors.
- Forging: Ring-rolled, upset and open-die from 5 kg to 3,000 kg, and typical use: Turbine discs, flanges, shafts, rings.
- Flange: ASME B16.5 / B16.47 in Class 150 through 2500, and typical use: Piping systems, pressure vessels, skids.
Related resources
Follow the links for the per-grade pages, the figures there match the ones on this page.
- semi finished forms, Inconel 718
- semi finished forms, Inconel 625
- semi finished forms, Hastelloy C-276
- semi finished forms, Hastelloy X
- semi finished forms, Monel 400
- semi finished forms, Nimonic 80A
- semi finished forms, Waspaloy
- semi finished forms, Nickel 200
- semi finished forms, MP35N
- semi finished forms, L605
- semi finished forms, 4J29
- semi finished forms, 4J36
- semi finished forms, 1J22
- semi finished forms, 1J50
- semi finished forms, Incoloy 800
- semi finished forms, Incoloy 800H
- semi finished forms, Incoloy 800HT
- semi finished forms, Incoloy 825
- semi finished forms, Incoloy 925
- semi finished forms, 3J21
- Inconel 718 sheet thickness guide
- Weight calculator by grade and form
- Stock forms by grade